The SEM images show that the particulates reinforcements (SiC and PKSA) were uniformly dispersed in the matrix. The percentage porosity for the composites ranged from 2.06 to 2.39%. In addition, hardness, yield strength and ultimate tensile strength of the composites are about 10.3%, 18.5% and 10.4%, respectively better than for Al 6063. However, the percent elongation and fracture toughness are lower for the hybrid composites than for Al 6063 and SiC reinforced composite with values decreasing with increase in ash content. Hence, the M