The goal of the work was to describe properties of asphalt-cement concrete (ACC) with reclaimed asphalt pavement (RAP), Portland cement, sand, and rubber powder (RP), as a material to base courses of road pavements. The mixtures were designed with the RAP in the amount of 75, 80, and 85% (m/m) and chosen cement-sand-rubber (CSR) mortar. Three CSR mortars were composed with cement CEM 42.5 R in the amount 29% (m/m); washed sand 0/2 mm in the amount 29, 35, or 41%; rubber powder of granulation 0/1 mm in the amount of 18, 24, or 29%