https://www.selleckchem.com/products/iwp-2.html
10 while Cd2+ (979 mg/g) and Cu2+ (877 mg/g) at the initial pH values of 4.14 and 6.13. High Ca(OH)2-bearing chitosan prepared from HCl and H2SO4 treated chtin showed the optimum Cd2+ (978 mg/g) and Cu2+ (852 mg/g) adsorption at an initial pH value of 2.10. Biosorption isotherm and kinetics models showed that the adsorption data of Pb2+, Cd2+ and Cu2+ onto the surface of chitosan was well-fitted by Langmuir model and Pseudo-second-order model with correlation coefficient (R2 0.95 and R2 0.91, respectively). Pseudo-second-order m