https://www.selleckchem.com/pr....oducts/o-pentagalloy
7% less than that prepared at 50% amplitude of ultrasonic irradiation. The particles of C60/Ga2O3 prepared by different modes of amplitude formed large (2-12 μm) aggregates in their solid phase.Whereas, in the aqueous medium, they were found to disperse in their nano sizes. The minimum particle size of the as-synthesized C60/Ga2O3 in an aqueous medium prepared by the proposed method of switching ultrasonic amplitude reached to approximately 467 nm. Comparatively, the minimum particle sizes were approximately 658 nm and 144