https://www.selleckchem.com/pr....oducts/Cytarabine(Cy
11 g/tex which is higher than untreated fibres with a breaking tenacity of 25.72 g/tex. The best properties were obtained in the sample with 4 layers of glass and 9 layers of sisal fibres using 200 ml of resin. The composite had a tensile strength of 57.60 MPa, flexural strength of 36 N/mm2, moisture absorption of 10% and a burning rate of 9.82 mm/min. These results were then compared with those of the current partition boards in the market. It was noted that the composite was suitable for use in partition boards. Again, r