https://www.selleckchem.com/products/arry-382.html
The results were assessed by using the paired t test and the Bland-Altman method (α=.05). RESULTS Mean 3D cement-gap thickness assessed by the triple-scan method reported small dispersion with a coefficient of variation of 5.6% for the occlusal area, 1.9% for the axial area, and 6.4% for the margin area. Cement gap thickness measured at corresponding locations in the aligned scan data sets and in the physical silicone replica reported no significant difference (P=.326) and good agreement. CONCLUSIONS The cement gap was accurately dupli