The lowest strength was observed in the samples after application of the plate without spraying and the pin with spraying of hydroxyapatite doped with silver (4 weeks), and the pin without spraying (8 weeks after implantation). The processes of integration of implants with spraying on their surface of the biocomposite with the surrounding bone were determined by electron microscopy. The advantage of intramedullary and bony fixators with spraying on the surface of the material based on bioactive glass, compared to osteosynthesi