https://www.selleckchem.com/pr....oducts/l-mimosine.ht
For all the studied self-adhesive cements, the failure of adhesion between the cement and dentin was predominant mode. Significant differences were found in the shear bond strengths of the CAD/CAM ceramics luted to dentin using tested self-adhesive and conventional cements. The bond strength depended on the combination of ceramic and cement. The IPS e.max ZirCAD had the highest bond strength to dentin after cementation with RelyX U200, while the IPS Empress CAD and IPS e.max CAD - with Panavia V5. Significant differences were found i