5 week ago - Translate

https://www.selleckchem.com/pr....oducts/srt2104-gsk22
The μSBS (mean ± standard deviation) values for groups SDF, SDF-KI, and SDF + GSH were 4.81 ± 2.026, 5.78 ± 1.809, 8.18 ± 2.828 megapascal respectively. Group 3 showed significantly better bond strength compared to groups 1 and 2. In group 2, the addition of KI showed better bond strength when compared to group 1, but the difference was not statistically significant. Pretreatment of teeth with GSH along with SDF application showed significantly better bond strength of GIC to CAD compared to SDF and SDF-KI. Pretreatment of tee