reated with 0.25 % graphene oxide and 3.8 % silver diamine fluoride when bonded to resin-modified glass ionomer cement. The application of methylene blue photosensitizer for photodynamic therapy undermined the adhesive bond strength applied on demineralized dentin. Improved bond strength and marginal microleakage scores were demonstrated by the demineralized dentin treated with 0.25 % graphene oxide and 3.8 % silver diamine fluoride when bonded to resin-modified glass ionomer cement. The application of methylene blue photosensitizer