3 day ago - Translate

https://www.selleckchem.com/products/ox04528.html
78 cN) than CL brackets (1967.38 cN) for the 1.6-3.0 deflection interval (p = 0.018). Within this interval, NiTi showed higher forces when used with CL brackets (2683.06 cN) than with SL brackets (1179.66 cN) (p  less then  0.0001). For the CL bracket systems, SS wires showed higher forces (2125.31 cN) in the 1.0-1.6 deflection interval than the other two wire alloys (NiTi, 1541.52 cN and GUMMETAL®, 852.65 cN) (p  less then  0.0001). SS wires also displayed lower forces with SL brackets (1844.01 cN) than in CL brackets (2125.31 cN) (p =