https://www.selleckchem.com/products/ABT-263.html
Finally, an in vitro bioactivity of the coatings was evaluated in a simulated body fluid solution at 37 °C. Results showed no apparent differences in the morphology and phase of the posttreated coatings, both of which are composed of a dense structure containing needle-like HA crystals. However, the HA-P/G-C/C sample possessed a higher Ca/P ratio and denser interface, thereby exhibiting higher adhesive performance and better bioactivity. The adhesive strength of the HA-P/G coating was observed at a critical load of 41.04 N, which increa