2 day ago - Translate

https://www.selleckchem.com/products/tpca-1.html
When the thickness of the printed layer is 0.3 mm, the printing path is 45°, and with vertical printing direction at a printing temperature of 525 °C, the bending strength of the sample reaches 159.2 MPa, which exceeds the bending performance of injection molded parts by 20%. It was also found that the greater the tensile strength of the printed specimen, the more uniform the size of each grain, and the higher the crystallinity of the material. The highest crystallinity exceeded 30%, which reached the crystallinity of injection molded pa