Though the F-GFA and G-GFA showcased higher water absorption ratio than the natural sand due to the presence of unreacted fly ash and GGBS particles, the complete replacement of fine aggregate with geopolymerized sand initiated the adequate compressive strength attainment up to 90% of natural sand, by reacting with the lime expelled out of the hydration process of cement in the mortar specimens developed in this experimental study. The geopolymer itself is hydrophilic in nature, and it will also aid for the higher water absorption ratio