The aim of this study was to assess monomer conversion, dimensional stability (mass and volume changes), biaxial flexural strength (BFS), and fluoride release of recently developed resin composites containing alkaline fillers (Cention N; CN) compared with resin-modified glass ionomer cements (RMGICs Riva LC; RL and Fuji II LC; FL), and conventional composite (Z35. FL showed highest monomer conversion (88±2%) followed by RL (73±10%), CN (59±2%), and Z350 (50±2%). RL exhibited highest mass and volume increase (10.22±0.04 wt% and 19.4±0